Skip to main content

Table 1 Mean particle size, size distribution (polidispersivity index, PDI), Zeta potential and encapsulation efficiency (EE) of empty PLGA NS and PTX-NS before and after freeze-drying.

From: Paclitaxel loading in PLGA nanospheres affected the in vitro drug cell accumulation and antiproliferative activity

 

Freeze-drying

Mean size (nm)

PDI

Zeta potential (mV)

% E.E.

PLGA NS

before

292.20 ± 72.50

0.385 ± 0.144

-5. 20 ± 0.10

-

 

after

386.76 ± 45.50

0.340 ± 0.150

-4. 60 ± 0.20

 

PTX-NS

before

192.00 ± 18.40

0.296 ± 0.071

-6.20 ± 0.20

35.59 ± 2.53

 

after

286.76 ± 45.50

0.340 ± 0.089

-5.10 ± 0.10

 
  1. Data are expressed as the mean ± SD of five separate experiments.